Abstract. Low-gradeilmenitecan be leached with concentrated HCl at atmospheric pressure and at 80 o C. After filtration to separate insoluble matter the solution containing TiO 2+ and Fe 2+ is heated to precipitate titanium hydroxide and recover HCl. The titanium hydroxide is then calcined to synthetic rutile containing 95+%TiO 2 while FeCl 2 is subjected to oxyhydrolysis or fluidized be to ...